During the period 1996–2006, the Communist Party of Nepal (Maoist) waged overt people’s war to seize state power and institute a new order that realized the party’s understanding of ‘New Democracy’ as posited by Mao Tse-tung. Contextual shifts led to a crucial strategic turning point in September 2005, when the Maoists agreed to a united front with estranged legal parties to oust the monarchy and establish a republic. Though touted as acceptance of political reintegration, the move was tactical rather than strategic. The party had no intention of supporting a parliamentary version of democracy and thus, 2006–2016, engaged in a covert effort to seize power. Central to this effort was the paramilitary Young Communist League (YCL), the members of which responded to inflammatory party verbiage and exhortations with attacks upon rival political actors. These attacks, academically and legally, were terrorism and offered a salient illustration of intra-state unrestricted warfare. Ultimately, organizational, national, and regional circumstances caused the main Maoist movement to move decisively away from its covert approach. By that time, however, radical splinters had embraced the use of terrorism against rival political actors, creating a situation whereby local politics is yet a dangerous endeavor in certain areas and at certain times.  相似文献   
2.
High nitrogen stainless steel with nitrogen content of 0.75%was welded by gas metal arc welding with Ar—N2-O2 ternary shielding gas. The effect of the ternary shielding gas on the retention and improvement of nitrogen content in the weld was identified. Surfacing test was conducted first to compare the ability of O2 and CO2 in prompting nitrogen dissolution. The nitrogen content of the surfacing metal with O2 is slightly higher than CO2. And then Ar—N2-O2 shielding gas was applied to weld high nitrogen stainless steel. After using N2-containing shielding gas, the nitrogen content of the weld was improved by 0.1 wt%. As N2 continued to increase, the increment of nitrogen content was not obvious, but the ferrite decreased from the top to the bottom. When the proportion of N2 reached 20%, a full austenitic weld was obtained and the tensile strength was improved by 8.7%. Combined with the results of surfacing test and welding test, it is concluded that the main effect of N2 is to inhibit the escape of nitrogen and suppress the ni-trogen diffusion from bottom to the top in the molten pool.  相似文献   
3.
用化学吸收光度法 (CAP)和热重 气相色谱联用法 (TG GC)测定了热分析逸出气中的氨。两种方法均简便、快捷和准确 ,通常回收率在 1 0 0± 6 %。比较了这些方法的使用范围  相似文献   
4.
基于模态分析的挠性接头角刚度测量研究   总被引:6,自引:0,他引:6       下载免费PDF全文
挠性接头是动力调谐陀螺的关键元件,刚度是其重要指标。针对挠性接头角刚度的测量,提出了一种基于模态分析的动态角刚度测量方法。该方法采用阶跃激励,利用高精度传感器和数据采集卡测量挠性接头的振动并采集数据,然后对采集数据进行数字滤波、FFT变换和频谱细化,计算出挠性接头的动态角刚度,同时相应地求出了角阻尼比系数。该方法解决了长期以来采用静态测试法测量挠性接头角刚度所带来的问题,具有测量精度高、操作方便、测试效率高、重复性好等特点。  相似文献   
1
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号